Severity of corrosion under insulation (CUI) to structures and strategies to detect it

<p>This review paper considers the research conducted in the past 30 years in the field of corrosion under insulation (CUI). CUI is a significant challenge in many industries for reasons of high cost and risk because it proceeds undetected under insulation. CUI is an unavoidable problem which...

وصف كامل

محفوظ في:
التفاصيل البيبلوغرافية
المؤلف الرئيسي: Elsadig O. Eltai (14586565) (author)
مؤلفون آخرون: Farayi Musharavati (14571268) (author), El-sadig Mahdi (14586566) (author)
منشور في: 2019
الموضوعات:
الوسوم: إضافة وسم
لا توجد وسوم, كن أول من يضع وسما على هذه التسجيلة!
_version_ 1864513563277656064
author Elsadig O. Eltai (14586565)
author2 Farayi Musharavati (14571268)
El-sadig Mahdi (14586566)
author2_role author
author
author_facet Elsadig O. Eltai (14586565)
Farayi Musharavati (14571268)
El-sadig Mahdi (14586566)
author_role author
dc.creator.none.fl_str_mv Elsadig O. Eltai (14586565)
Farayi Musharavati (14571268)
El-sadig Mahdi (14586566)
dc.date.none.fl_str_mv 2019-09-20T00:00:00Z
dc.identifier.none.fl_str_mv 10.1515/corrrev-2018-0102
dc.relation.none.fl_str_mv https://figshare.com/articles/journal_contribution/Severity_of_corrosion_under_insulation_CUI_to_structures_and_strategies_to_detect_it/22047749
dc.rights.none.fl_str_mv CC BY 4.0
info:eu-repo/semantics/openAccess
dc.subject.none.fl_str_mv Engineering
Materials engineering
Mechanical engineering
coatings
corrosive species
CUI
detection techniques
dc.title.none.fl_str_mv Severity of corrosion under insulation (CUI) to structures and strategies to detect it
dc.type.none.fl_str_mv Text
Journal contribution
info:eu-repo/semantics/publishedVersion
text
contribution to journal
description <p>This review paper considers the research conducted in the past 30 years in the field of corrosion under insulation (CUI). CUI is a significant challenge in many industries for reasons of high cost and risk because it proceeds undetected under insulation. CUI is an unavoidable problem which may potentially cause personnel injury or even fatalities. Presently, CUI counts for as much as 40 to 60% of pipeline-repairing cost. The use of coating under the insulation has been shown very efficient in the mitigation of CUI. Moisture and ion penetration, particularly chlorides, through the insulation and coating may produce stress corrosion cracking of austenitic stainless steels. The process of applying insulating materials on metal surfaces and the precautions that need to be taken are explained. Beside visual inspection, techniques such as neutron backscatter, capacitive imaging and pulsed eddy current can be used to detect the presence of CUI. The strength and limitations of the available commercial detection techniques are evaluated. A comprehensive list of industrial standards dealing with CUI is provided. </p> <h2>Other information</h2> <p>Published in: Corrosion Reviews<br> License: <a href="http://creativecommons.org/licenses/by/4.0" target="_blank">http://creativecommons.org/licenses/by/4.0</a><br> See article on publisher's website: <a href="http://dx.doi.org/10.1515/corrrev-2018-0102" target="_blank">http://dx.doi.org/10.1515/corrrev-2018-0102</a></p>
eu_rights_str_mv openAccess
id Manara2_134bec5a747c6ac4bc1f45a70e85cd11
identifier_str_mv 10.1515/corrrev-2018-0102
network_acronym_str Manara2
network_name_str Manara2
oai_identifier_str oai:figshare.com:article/22047749
publishDate 2019
repository.mail.fl_str_mv
repository.name.fl_str_mv
repository_id_str
rights_invalid_str_mv CC BY 4.0
spelling Severity of corrosion under insulation (CUI) to structures and strategies to detect itElsadig O. Eltai (14586565)Farayi Musharavati (14571268)El-sadig Mahdi (14586566)EngineeringMaterials engineeringMechanical engineeringcoatingscorrosive speciesCUIdetection techniques<p>This review paper considers the research conducted in the past 30 years in the field of corrosion under insulation (CUI). CUI is a significant challenge in many industries for reasons of high cost and risk because it proceeds undetected under insulation. CUI is an unavoidable problem which may potentially cause personnel injury or even fatalities. Presently, CUI counts for as much as 40 to 60% of pipeline-repairing cost. The use of coating under the insulation has been shown very efficient in the mitigation of CUI. Moisture and ion penetration, particularly chlorides, through the insulation and coating may produce stress corrosion cracking of austenitic stainless steels. The process of applying insulating materials on metal surfaces and the precautions that need to be taken are explained. Beside visual inspection, techniques such as neutron backscatter, capacitive imaging and pulsed eddy current can be used to detect the presence of CUI. The strength and limitations of the available commercial detection techniques are evaluated. A comprehensive list of industrial standards dealing with CUI is provided. </p> <h2>Other information</h2> <p>Published in: Corrosion Reviews<br> License: <a href="http://creativecommons.org/licenses/by/4.0" target="_blank">http://creativecommons.org/licenses/by/4.0</a><br> See article on publisher's website: <a href="http://dx.doi.org/10.1515/corrrev-2018-0102" target="_blank">http://dx.doi.org/10.1515/corrrev-2018-0102</a></p>2019-09-20T00:00:00ZTextJournal contributioninfo:eu-repo/semantics/publishedVersiontextcontribution to journal10.1515/corrrev-2018-0102https://figshare.com/articles/journal_contribution/Severity_of_corrosion_under_insulation_CUI_to_structures_and_strategies_to_detect_it/22047749CC BY 4.0info:eu-repo/semantics/openAccessoai:figshare.com:article/220477492019-09-20T00:00:00Z
spellingShingle Severity of corrosion under insulation (CUI) to structures and strategies to detect it
Elsadig O. Eltai (14586565)
Engineering
Materials engineering
Mechanical engineering
coatings
corrosive species
CUI
detection techniques
status_str publishedVersion
title Severity of corrosion under insulation (CUI) to structures and strategies to detect it
title_full Severity of corrosion under insulation (CUI) to structures and strategies to detect it
title_fullStr Severity of corrosion under insulation (CUI) to structures and strategies to detect it
title_full_unstemmed Severity of corrosion under insulation (CUI) to structures and strategies to detect it
title_short Severity of corrosion under insulation (CUI) to structures and strategies to detect it
title_sort Severity of corrosion under insulation (CUI) to structures and strategies to detect it
topic Engineering
Materials engineering
Mechanical engineering
coatings
corrosive species
CUI
detection techniques