Accelerated corrosion of stainless steel and Ni-based alloys in molten NaNO<sub>3</sub>-KNO<sub>3</sub> salt vapour phases
<p dir="ltr">The corrosion behaviour of four commonly used corrosion-resistant alloys in eutectic nitrate salt (NaNO<sub>₃</sub>/KNO<sub>₃</sub>) and its vapour phase was examined at 565 °C for 28 days. The findings revealed significantly higher corrosion rate...