1
Experimental study on effective placement of PCM packets in cooling vest to improve performance in warm environment
منشور في 2017"…The used PCM melting temperature is 28 °C with a coverage area of 642 cm2 and total weight of the vest of 1.19 kg including 8 PCM packets (87.5 grams each). …"
احصل على النص الكامل
احصل على النص الكامل
-
2
Thermal properties of phase-change materials based on high-density polyethylene filled with micro-encapsulated paraffin wax for thermal energy storage
منشور في 2015"…The thickness of the shell was approximately 1.5 μm. Shape-stabilized phase change materials (PCM) based on high-density polyethylene (HDPE) mixed with micro-encapsulated paraffin wax were prepared and investigated for application in thermal energy storage. …"
احصل على النص الكامل
احصل على النص الكامل
احصل على النص الكامل