Showing 1 - 14 results of 14 for search '(((( i x decrease ) OR ( _ wt decrease ))) OR ( 5 _ decrease ))~', query time: 0.10s Refine Results
  1. 1

    Structural, wear and thermal behaviour of Cu–Al2O3–graphite hybrid metal matrix composites by Mittal, P.

    Published 2020
    “…Copper matrix composites with Al2O3–graphite reinforcement (0.5-0.5, 1.0-1.0, 1.5-1.5 and 2.0-2.0 wt%) were prepared by stir casting process. …”
    Get full text
    Get full text
  2. 2

    Synthesis and characterisation of Co2+-incorporated ZnO nanoparticles prepared through a sol-gel method by Ba-Abbad, Muneer M.

    Published 2016
    “…The band gap of the Co2+-doped ZnO samples decreased from 3.19 to 2.66 eV as the content of dopant Co2+ increased from 0.0 to 1.0 wt.%. …”
    Get full text
    Get full text
  3. 3

    Synthesis and characterization of stir casted Cu-ZrO2-Graphite hybrid metal matrix composites for thermal management structures by Mittal, Prateek

    Published 2022
    “…ZrO2 and Graphite reinforcements were added (0.5–0.5, 1.0–1.0, 1.51.5 and 2.0–2.0 wt %) in the four composite samples prepared via stir casting. …”
    Get full text
    Get full text
    Get full text
  4. 4

    Enhanced quality factor of polyvinyl formal (PVF) based nanocomposites filled with zinc oxide and carbon black nanoparticles for wireless sensing applications by Mohanapriya, M.K.

    Published 2019
    “…The incorporation of ZnO at 10% decreases Q-factor to 36.1. Incorporation of CBNP at 5% and ZnO at 5% further reduces the Q-factor to 13.7. …”
    Get full text
    Get full text
  5. 5

    Morphology, nucleation, and isothermal crystallization kinetics of poly(butylene succinate) mixed with a polycarbonate/MWCNTs masterbatch by Gumede, Thandi P.

    Published 2018
    “…The nanocomposites contained 0.5, 1.0, 2.0, and 4.0 wt% MWCNTs. Differential scanning calorimetry (DSC), small angle X-ray scattering (SAXS) and wide angle X-ray scattering (WAXS) results indicate that the blends are partially miscible, hence they form two phases (i.e., PC-rich and PBS-rich phases). …”
    Get full text
    Get full text
  6. 6

    Morphology, Nucleation, and Isothermal Crystallization Kinetics of Poly(ε-caprolactone) Mixed with a Polycarbonate/MWCNTs Masterbatch by Gumede, Thandi P.

    Published 2017
    “…The nanocomposites contained 0.5, 1.0, 2.0, and 4.0 wt % MWCNTs. Even though PCL and PC have been reported to be miscible, our DSC (Differential Scanning Calorimetry), SAXS (Small Angle X-ray Scattering), and WAXS (Wide Angle X-ray Scattering) results showed partial miscibility, where two phases were formed (PC-rich and PCL-rich phases). …”
    Get full text
    Get full text
  7. 7

    Synthesis and properties of HA/ZnO/CNT nanocomposite by Ding M.

    Published 2018
    “…The goal of this study was to examine the tribomechanical properties of hydroxyapatite (HA)/ZnO and HA/ZnO/CNT composite ceramics (carbon nanotubes; with different ratios 0.5 wt%, 1.0 wt%, and 1.5 wt%). The composites were synthesized using the hydrothermal method in an autoclave. …”
    Get full text
    Get full text
  8. 8

    Phase, microstructure and tensile strength of Al–Al2O3–C hybrid metal matrix composites by Ahamad, N.

    Published 2020
    “…Aluminium matrix reinforced with Al2O3–carbon (2.5, 5, 7.5 and 10 wt.%) in equal proportion was prepared by stir casting. …”
    Get full text
    Get full text
  9. 9

    Structural and mechanical characterization of stir cast Al–Al2O3–TiO2 hybrid metal matrix composites by Ahamad, N.

    Published 2020
    “…Aluminium matrix reinforced with aluminium oxide?titanium oxide (2.5, 5.0, 7.5 and 10 wt.%) in equal proportion were prepared by stir casting. …”
    Get full text
    Get full text
  10. 10
  11. 11
  12. 12

    Modified zno nanoparticles using iron ions (Fe3+) for photo-catalytic degradation of toxic pollutants under sunlight by Ba-Abbad, Muneer M.

    Published 2019
    “…As the Fe3+ concentration increased from 0.25 to 1.00 wt. %, the crystal size decreased in comparison with the undoped ZnO. …”
    Get full text
  13. 13

    Effect of electroless bath composition on the mechanical, chemical, and electrochemical properties of new NiP-C 3 N 4 nanocomposite coatings by Fayyad E.M.

    Published 2019
    “…An electroless bath of 0.5 g L−1 C3N4 offered a nanocomposite coating with the highest microhardness and superior corrosion resistance. …”
    Get full text
    Get full text
  14. 14

    Enhancing the corrosion resistance of reinforcing steel under aggressive operational conditions using behentrimonium chloride by Radwan A.B.

    Published 2019
    “…Using only a 50 ?mol L?1 of BTC, we are able to measure an inhibition efficiency of 91, 79, and 71% in SCP solution with 3.5% NaCl at pH of 12.5, 10 and 7, respectively without showing any effect on the mechanical properties on the cured mortars. …”
    Get full text
    Get full text