    Microstructure, wear and corrosion characteristics of Cu matrix reinforced SiC–graphite hybrid composites by Jamwal A.

    Published 2019
    “…Copper matrix composites with SiC-graphite reinforcement (0, 2.5,5, 7.5 and 10 wt.%) were prepared by stir casting process. …”
    Get full text
    Get full text
  5. 5
  6. 6
  7. 7

    Structural, wear and thermal behaviour of Cu–Al2O3–graphite hybrid metal matrix composites by Mittal, P.

    Published 2020
    “…Copper matrix composites with Al2O3–graphite reinforcement (0.5-0.5, 1.0-1.0, 1.5-1.5 and 2.0-2.0 wt%) were prepared by stir casting process. …”
    Get full text
    Get full text
  8. 8
  9. 9

    Synthesis and characterization of stir casted Cu-ZrO2-Graphite hybrid metal matrix composites for thermal management structures by Mittal, Prateek

    Published 2022
    “…ZrO2 and Graphite reinforcements were added (0.5–0.5, 1.01.0, 1.5–1.5 and 2.0–2.0 wt %) in the four composite samples prepared via stir casting. …”
    Get full text
    Get full text
    Get full text
  10. 10

    Influence of nitrogen doping on the electrocatalytic activity of Ni-incorporated carbon nanofibers toward urea oxidation by Barakat, Nasser A.M.

    Published 2017
    “…However, the electrochemical measurements indicated that the content of the urea in the initial electrospun solution should be optimized as the results showed that the best nickel surface activation as well as the maximum observed current density can be achieved when the urea content is kept at 5 wt%. Typically, the observed current densities using 1.0 M urea (in 1 M KOH) were 3.15, 29.7, 13.75, 47.55, 14.13 and 9.85 mA/cm2 for the nanofibers obtained from electrospun solutions having 0, 1, 2, 5, 7 and 9 wt% urea, respectively. …”
    Get full text
    Get full text
  11. 11

    Production and investigation of flexible nanofibers of sPEEK/PVP loaded with RuO2 nanoparticles by Chamakh, Mariem

    Published 2021
    “…The samples were synthesized with different concentrations of hydrous ruthenium chloride of 2 wt%, 5 wt%, and 10 wt%, and then annealed at a temperature of 300 �C for 4 h to form the ruthenium oxide nanoparticles. …”
    Get full text
    Get full text
  12. 12
  13. 13
  14. 14

    Enhanced quality factor of polyvinyl formal (PVF) based nanocomposites filled with zinc oxide and carbon black nanoparticles for wireless sensing applications by Mohanapriya, M.K.

    Published 2019
    “…The incorporation of ZnO at 10% decreases Q-factor to 36.1. Incorporation of CBNP at 5% and ZnO at 5% further reduces the Q-factor to 13.7. …”
    Get full text
    Get full text
  15. 15

    Synthesis and characterisation of Co2+-incorporated ZnO nanoparticles prepared through a sol-gel method by Ba-Abbad, Muneer M.

    Published 2016
    “…The band gap of the Co2+-doped ZnO samples decreased from 3.19 to 2.66 eV as the content of dopant Co2+ increased from 0.0 to 1.0 wt.%. …”
    Get full text
    Get full text
  16. 16
  17. 17

    Effect of concentration of DOC loaded TiO 2 nanotubes on the corrosion behavior of smart coatings by Ubaid F.

    Published 2019
    “…Various contents of the encapsulated TiO2 nanotubes (1, 3 and 5wt%) were thoroughly dispersed into the epoxy matrix and the resulting composites were then applied on a cleaned steel substrate using doctor blade technique to develop smart coatings. …”
    Get full text
    Get full text
  18. 18
  19. 19

    Tailoring electrocatalytic properties of Pt nanoparticles grown on Ti3C2Tx MXene surface by Filip, Jaroslav

    Published 2019
    “…Composites containing 14 wt% Pt showed HER with an onset potential of −75.9 mV and a current density of −10 mA cm−2 achieved at −226 mV. …”