Search alternatives:
values decrease » values increased (Expand Search), largest decrease (Expand Search)
large decrease » marked decrease (Expand Search), large increases (Expand Search), large degree (Expand Search)
8 cycles » _ cycles (Expand Search), 6 cycles (Expand Search), 10 cycles (Expand Search)
i large » _ large (Expand Search), a large (Expand Search), via large (Expand Search)
values decrease » values increased (Expand Search), largest decrease (Expand Search)
large decrease » marked decrease (Expand Search), large increases (Expand Search), large degree (Expand Search)
8 cycles » _ cycles (Expand Search), 6 cycles (Expand Search), 10 cycles (Expand Search)
i large » _ large (Expand Search), a large (Expand Search), via large (Expand Search)
-
101
-
102
-
103
Decreased CNPase levels in the SG/RC in <i>Large</i><sup><i>myd/myd</i></sup> <i>mice</i>.
Published 2020“…<p>Lysates were obtained from the spiral ganglion (SG)/Rosenthal’s canal (RC) of the P5-7 control and <i>Large</i><sup><i>myd/myd</i></sup> mice. CNPase immunoblotting showed decreased levels of CNPase in the <i>Large</i><sup><i>myd/myd</i></sup> mice. …”
-
104
-
105
-
106
-
107
-
108
-
109
Table 1_Quantitative characterization of damage and the cross-scale evolution mechanism of soft rock under dry-wet cycles.xlsx
Published 2024“…The study results indicate that soft rock exhibits a random fractal damage effect under the action of dry–wet cycles. As the number of cycles increases, the multifractal spectrum becomes more asymmetric and the discretization degree becomes more uneven. …”
-
110
-
111
-
112
-
113
Experimental investigations on the durability of flowable fill under drying-wetting and freeze-thaw actions and its implica-tions for highway constructions
Published 2022“…After six drying-wetting cycles, the specimens showed 27 – 51% strength reduction as compared to their counterparts with no drying-wetting actions. …”
-
114
-
115
-
116
-
117
-
118
-
119
Glass beads.
Published 2024“…Secondly, the concrete variable angle shear test was carried out under the temperature and humidity cycle, which revealed that the shear strength of thermal insulated shotcrete increased firstly and then decreased with the increase of temperature at the same number of cycles. …”
-
120
Limestone particles.