يعرض 1 - 1 نتائج من 1 نتيجة بحث عن '(( 10 ((greater decrease) OR (((_ decrease) OR (a decrease)))) ) OR ( 30 min decrease ))~', وقت الاستعلام: 0.12s تنقيح النتائج
  1. 1

    Effect Of Sand Blasting On Soda Lime Glass Properties حسب Bousbaa, C.

    منشور في 2003
    "…The average strength remains almost constant while the dispersion becomes much reduced for the glass sand blasted during 60 minutes (m = 10.4 and smoy = 64 MPa). The variation of the relative efficiency of glass protected solar panels versus sand blasting duration (seen up to 300 min) shows a slow regular decrease until 0.91 for a 90° impact angle and until 0.95 for 30°. …"