    Experimental investigation on the compressibility of Al/Al2O3 nanocomposites حسب Wagih, Ahmed

    منشور في 2016
    "…The results showed that the grain size of milled powders was about 43 nm with a noticeable presence of agglomerates at 10 wt.% of Al2O3. By increasing Al2O3 weight fraction to 12% the decrease in grain size was very. …"
    احصل على النص الكامل
    احصل على النص الكامل
  9. 9
  10. 10
  11. 11
  12. 12
  13. 13

    The Impact of COVID-19 on Physical (In)Activity Behavior in 10 Arab Countries حسب Al Sabbah, Haleama

    منشور في 2022
    "…This study aimed to assess the impact of COVID-19 on physical (in)activity behavior in 10 Arab countries before and during the lockdown. …"
    احصل على النص الكامل
    احصل على النص الكامل
  14. 14

    Phase, microstructure and tensile strength of Al–Al2O3–C hybrid metal matrix composites حسب Ahamad, N.

    منشور في 2020
    "…Aluminium matrix reinforced with Al2O3–carbon (2.5, 5, 7.5 and 10 wt.%) in equal proportion was prepared by stir casting. …"
    احصل على النص الكامل
    احصل على النص الكامل
  15. 15
  16. 16
  17. 17
  18. 18
  19. 19

    Improved properties of Al-Si3N4 nanocomposites fabricated through a microwave sintering and hot extrusion process حسب Matli, Penchal Reddy

    منشور في 2017
    "…In this study, nano-sized Si3N4 (0, 0.5, 1.0 and 1.5 vol%)/Al composites were fabricated using a powder metallurgy method involving microwave sintering technique followed by hot extrusion. …"
    احصل على النص الكامل
    احصل على النص الكامل
  20. 20

    Effect of reinforcement concentration on the properties of hot extruded Al-Al2O3 composites synthesized through microwave sintering process حسب Reddya, M. Penchal

    منشور في 2017
    "…In this study, Aluminum matrix composite reinforced with 5, 10 and 15 vol% Al2O3 particles were fabricated using microwave assisted rapid sintering technique followed by hot extrusion. …"