    Effect of anions on the structural, morphological and dielectric properties of hydrothermally synthesized hydroxyapatite nanoparticles حسب Sundarabharathi L.

    منشور في 2020
    "…For the particles obtained from nitrate, acetate, chloride and egg shell precursors respectively give dielectric constant (εʹ) values of 9.96, 13.22, 9.92 and 10.86 at 5 MHz. The εʹ and dielectric loss (εʹʹ) values for the HA nanoparticles decrease with increase in the applied frequency as well. …"
    احصل على النص الكامل
    احصل على النص الكامل
  3. 1003
  4. 1004

    Synthesis and characterization of nanocrystalline CoFe2O4-zirconia via propylene oxide aided sol-gel method حسب Bhosale R.R.

    منشور في 2018
    "…The prepared gels were aged, dried, and annealed at different temperatures (600 1000 C) and times (1 5 h). The annealed Co ferrite/ZrO2 powder was analyzed by powder X-ray diffraction (PXRD), Brunauer Emmett Teller surface area analysis, energy-dispersive spectroscopy (EDS), scanning electron microscopy (SEM), and transmission electron microscopy (TEM). …"
    احصل على النص الكامل
    احصل على النص الكامل
  5. 1005
  6. 1006
  7. 1007
  8. 1008
  9. 1009
  10. 1010
  11. 1011
  12. 1012

    Effect of concentration of DOC loaded TiO 2 nanotubes on the corrosion behavior of smart coatings حسب Ubaid F.

    منشور في 2019
    "…Towards this direction, TiO2 nanotubes with an average size of ⁓10–15 nm (as confirmed by scanning electron microscope (SEM) and transmission electron microscope (TEM) analysis) were synthesized through a hydrothermal process and were then impregnated with DOC. …"
    احصل على النص الكامل
    احصل على النص الكامل
  13. 1013
  14. 1014
  15. 1015
  16. 1016

    The mechanical and adhesive properties of electrically and thermally conductive polymeric composites based on high density polyethylene filled with nickel powder حسب Krupa, Igor

    منشور في 2013
    "…The stress at break of the composites behaved nonlinearly; the low filler content suppressed necking, resulting in a decrease in stress at break, whereas higher filler content (higher than 10vol.%) led to reinforcement of the composites and therefore increased the stress at break.The presence of nickel particles throughout the HDPE matrix increased the hydrophilicity of the composites. …"
    احصل على النص الكامل
    احصل على النص الكامل
    احصل على النص الكامل
  17. 1017
  18. 1018
  19. 1019

    Bond durability of sand coated and ribbed basalt FRP bars embedded in high-strength concrete حسب Al-Hamrani, Abathar

    منشور في 2023
    "…However, specimens with high-strength concrete achieved most of or above their maximum bond strength after the descending stage, while those with normal-strength concrete showed a decrease in bond strength to an approximately constant value with continuous slip. …"
    احصل على النص الكامل
    احصل على النص الكامل
  20. 1020

    Production and investigation of flexible nanofibers of sPEEK/PVP loaded with RuO2 nanoparticles حسب Chamakh, Mariem

    منشور في 2021
    "…The samples were synthesized with different concentrations of hydrous ruthenium chloride of 2 wt%, 5 wt%, and 10 wt%, and then annealed at a temperature of 300 �C for 4 h to form the ruthenium oxide nanoparticles. …"
    احصل على النص الكامل
    احصل على النص الكامل