    Experimental results and modelling of corrosion-damaged concrete beams strengthened with externally-bonded composites حسب Elghazy M.

    منشور في 2018
    "…The investigated parameters included the corrosion levels (10 and 20% mass loss of steel reinforcement), the type of composite (fabric-reinforced cementitious matrix (FRCM) and fiber-reinforced polymers (FRP)), and the number of composite layers (one, two, and four). …"
    احصل على النص الكامل
    احصل على النص الكامل
  3. 543
  4. 544

    The Expression of TBC1 Domain Family, Member 4 (TBC1D4) in Skeletal Muscles of Insulin-Resistant Mice in Response to Sulforaphane حسب Rizk, Nasser M

    منشور في 2020
    "…Thereafter, DIO mice received either SFN (5mg/kg BW) (n=10) or vehicle (n=10) as controls daily by intraperitoneal injections for four weeks. …"
    احصل على النص الكامل
    احصل على النص الكامل
  5. 545
  6. 546
  7. 547
  8. 548
  9. 549
  10. 550
  11. 551
  12. 552
  13. 553
  14. 554
  15. 555
  16. 556

    Recycled Waste Tires Management in Constructions حسب Hamid, Salma Mohamed

    منشور في 2020
    "…The LCCA results show that the rubberized concrete (RC2), obtained by replacing 5% of aggregate and mixing it with seawater, is more cost-effective than RC1, with a cost savings of 30%.LCCA data were acquired by investigating thirteen concrete mixes (a control mix; 5%, 10%, and 20% rubber aggregate substitutions mixed with freshwater; and 0%, 5%, and 10% rubber aggregate substitutions mixed with seawater). …"
    احصل على النص الكامل
  17. 557
  18. 558

    Enhanced bioelectrochemical treatment of petroleum refinery wastewater with Labaneh whey as co-substrate حسب Mohanakrishna, Gunda

    منشور في 2020
    "…On the contrary, a maximum substrate degradation rate of 0.420 kg COD/m3-day (ξCOD, 63.10%), was registered with 80:20 feed. Higher LW ratios in PRW lead to the production of VFA which in turn gradually decreased the anolyte pH to below 4.5 (70:30 feed). …"
    احصل على النص الكامل
    احصل على النص الكامل
    احصل على النص الكامل
  19. 559

    Morphology, nucleation, and isothermal crystallization kinetics of poly(butylene succinate) mixed with a polycarbonate/MWCNTs masterbatch حسب Gumede, Thandi P.

    منشور في 2018
    "…The nanocomposites contained 0.5, 1.0, 2.0, and 4.0 wt% MWCNTs. Differential scanning calorimetry (DSC), small angle X-ray scattering (SAXS) and wide angle X-ray scattering (WAXS) results indicate that the blends are partially miscible, hence they form two phases (i.e., PC-rich and PBS-rich phases). …"