    Microstructure Evolution of the Mg-5.8 Zn-0.5 Zr-1.0 Yb Alloy During Homogenization by Lu Li (14069)

    Published 2022
    “…After homogenization, most of the eutectic phases dissolve into the matrix, except for a small amount of Mg-Zn-Yb phase. The area fractions of residual secondary phase decrease from 5.54% in the as-cast alloy to 0.59% in the well-homogenized sample. …”