    Phase, microstructure and tensile strength of Al–Al2O3–C hybrid metal matrix composites by Ahamad, N.

    Published 2020
    “…Scanning electron microscopy shows that Al matrix has uniform distribution of reinforcement particles, i.e. Al2O3 and carbon. Density decreases due to variation of reinforcement because ceramic reinforcement has low density. …”
    Get full text
    Get full text
  3. 3

    Correlation of structural and mechanical properties for Al-Al2O3-SiC hybrid metal matrix composites by Ahamad, Naseem

    Published 2021
    “…Hardness of hybrid composites increases upto 5 wt.% variation of ceramic reinforcements i.e. …”
    Get full text
    Get full text
  4. 4
  5. 5
  6. 6
  7. 7

    Improved mechanical properties of recycled linear low-density polyethylene composites filled with date palm wood powder by AlMaadeed, Mariam A.

    Published 2014
    “…The ratio between the stress at break at 25°C versus 50°C (σ25/σ50) was between 2.7 and 3.8, whereas the ratio of Young’s modulus of E25/E50 was between 1.6 and 2.6.…”
    Get full text
    Get full text
    Get full text
  8. 8
  9. 9

    Enhancing the corrosion resistance of reinforcing steel under aggressive operational conditions using behentrimonium chloride by Radwan A.B.

    Published 2019
    “…Herein, the inhibition efficiency of a new corrosion inhibitor, behentrimonium chloride (BTC, C25H54ClN), is explored in a simulated-concrete pore solution (SCP) with 3.5 wt.% NaCl at different pH using electrochemical impedance spectroscopy (EIS) and polarization methods. …”