    Effect of copper-nickel interlayer thickness on laser welding-brazing of Mg/Ti alloy حسب Auwal, S.T.

    منشور في 2019
    "…In comparison, a mixed interfacial reaction layer consisted of Ti2Ni and Ti3Al was formed from the direct irradiation zone to the weld toe zone of the joint with comparable Ni and Cu coating thicknesses (10.78 µm Cu–9.30 µm Ni). In this case, the thickness of the mixed layer was below the critical thickness of 10 µm. …"