    Influence of nitrogen doping on the electrocatalytic activity of Ni-incorporated carbon nanofibers toward urea oxidation by Barakat, Nasser A.M.

    Published 2017
    “…Typically, the observed current densities using 1.0 M urea (in 1 M KOH) were 3.15, 29.7, 13.75, 47.55, 14.13 and 9.85 mA/cm2 for the nanofibers obtained from electrospun solutions having 0, 1, 2, 5, 7 and 9 wt% urea, respectively. …”
    Get full text
    Get full text
  8. 468

    Corrosion inhibition of Mild Steel at Elevated temperature in highly Acidic Brines using a green corrosion inhibitor by Elhaddad, Muhsen A.M.

    Published 2017
    “…Corrosion Inhibition of mild steel in 5 M Hydrochloric acid solution at different temperatures was investigated using a new green corrosion inhibitor (lauramidopropylamine oxide). …”
    Get full text
  9. 469

    Removal of toxic pollutants from produced water by phytoremediation: Applications and mechanistic study by Atia, Fathy A.M.

    Published 2019
    “…Results showed that except M. sativa, tolerated up to 10% diluted PW with a 30% decrease in length and biomass compared to control treatment, all other plants could not survive. …”
    Get full text
    Get full text
    Get full text
  10. 470

    Removal of toxic pollutants from produced water by phytoremediation: Applications and mechanistic study by Fathy A.M., Atia

    Published 2019
    “…Results showed that except M. sativa, tolerated up to 10% diluted PW with a 30% decrease in length and biomass compared to control treatment, all other plants could not survive. …”
    Get full text
    Get full text
    Get full text
  11. 471

    Magnetorheological elastomer-based variable stiffness flexible coupling for vibration isolation by Syam, Thaer M.I.

    Published 2021
    “…Our results show that the level of vibration decreased when the magnetic field increased. The first natural frequency of the system happened at 26 Hz and moved to 28 Hz when the applied magnetic field increased from 0 to 12.38 mT. …”
    Get full text
    Get full text
  12. 472
  13. 473
  14. 474

    Arabic gum as green agent for ZnO nanoparticles synthesis: properties, mechanism and antibacterial activity by Ba-Abbad, Muneer M.

    Published 2017
    “…The size of the spherically shaped ZnO NPs decreased with an increase in the amount of Arabic gum, up to an optimal 1.50 wt%. …”
    Get full text
    Get full text
  15. 475

    Prospects Of Amino Acids And Ionic Liquids As Natural Gas Hydrate Inhibitors For Offshore Flow Assurance by Qureshi, M. Fahed Aziz

    Published 2018
    “…The effect of stirring on the hydrate crystal formation at different stirring rates (100-1400 RPM) was also investigated. It was found that a threshold limit exists for the stirring rate, above and below which no hydrate formation is likely to occur within the selected system. …”
    Get full text
  16. 476

    Improved mechanical properties of recycled linear low-density polyethylene composites filled with date palm wood powder by AlMaadeed, Mariam A.

    Published 2014
    “…The Young’s modulus and stress at break measured at 50°C decreased significantly compared with those values measured at 25°C. …”
    Get full text
    Get full text
    Get full text
  17. 477

    Cobalt phthalocyanine as a novel molecular recognition reagent for batch and flow injection potentiometric and spectrophotometric determination of anionic surfactants by El-Nemma, Eman M.

    Published 2008
    “…The maximum absorption of the reagent at 658 nm linearly decreases with the increase of anionic surfactant over the concentration range 2–30 μg mL−1. …”
    Get full text
    Get full text
  18. 478
  19. 479

    Synthesis and electrochemical properties of nickel oxide/carbon nanofiber composites by Al-Enizi, Abdullah M.

    Published 2014
    “…The specific capacitance (SC) was found to be highest (738 F g−1) at a calcination temperature of 400 °C. The charge transfer resistance (Rp) decreased as the calcination temperature was increased. …”