Showing 37,641 - 37,660 results of 109,976 for search '(( a point decrease ) OR ( 5 ((step decrease) OR (((mean decrease) OR (a decrease)))) ))', query time: 1.94s Refine Results
  1. 37641

    Technical indicators of coarse aggregate. by Yining Wang (432154)

    Published 2025
    “…Experimental results show that the ZM modifier significantly improves the dynamic stability and rutting resistance of the mixture, with dynamic stability increasing to 5245 and rut depth decreasing to 2.26 mm at a dosage of 0.5%. The low-temperature flexural strain increases while the bending stiffness decreases, indicating improved crack resistance. …”
  2. 37642

    Technical specifications of fine aggregates. by Yining Wang (432154)

    Published 2025
    “…Experimental results show that the ZM modifier significantly improves the dynamic stability and rutting resistance of the mixture, with dynamic stability increasing to 5245 and rut depth decreasing to 2.26 mm at a dosage of 0.5%. The low-temperature flexural strain increases while the bending stiffness decreases, indicating improved crack resistance. …”
  3. 37643

    Rutting test results of asphalt mixtures. by Yining Wang (432154)

    Published 2025
    “…Experimental results show that the ZM modifier significantly improves the dynamic stability and rutting resistance of the mixture, with dynamic stability increasing to 5245 and rut depth decreasing to 2.26 mm at a dosage of 0.5%. The low-temperature flexural strain increases while the bending stiffness decreases, indicating improved crack resistance. …”
  4. 37644

    Gradation composition of asphalt mixture. by Yining Wang (432154)

    Published 2025
    “…Experimental results show that the ZM modifier significantly improves the dynamic stability and rutting resistance of the mixture, with dynamic stability increasing to 5245 and rut depth decreasing to 2.26 mm at a dosage of 0.5%. The low-temperature flexural strain increases while the bending stiffness decreases, indicating improved crack resistance. …”
  5. 37645

    Results of the orthogonal test. by Yining Wang (432154)

    Published 2025
    “…Experimental results show that the ZM modifier significantly improves the dynamic stability and rutting resistance of the mixture, with dynamic stability increasing to 5245 and rut depth decreasing to 2.26 mm at a dosage of 0.5%. The low-temperature flexural strain increases while the bending stiffness decreases, indicating improved crack resistance. …”
  6. 37646

    Rutting test results. by Yining Wang (432154)

    Published 2025
    “…Experimental results show that the ZM modifier significantly improves the dynamic stability and rutting resistance of the mixture, with dynamic stability increasing to 5245 and rut depth decreasing to 2.26 mm at a dosage of 0.5%. The low-temperature flexural strain increases while the bending stiffness decreases, indicating improved crack resistance. …”
  7. 37647

    Technical Specifications of ZM Modifier. by Yining Wang (432154)

    Published 2025
    “…Experimental results show that the ZM modifier significantly improves the dynamic stability and rutting resistance of the mixture, with dynamic stability increasing to 5245 and rut depth decreasing to 2.26 mm at a dosage of 0.5%. The low-temperature flexural strain increases while the bending stiffness decreases, indicating improved crack resistance. …”
  8. 37648

    Gradation curve of asphalt mixture. by Yining Wang (432154)

    Published 2025
    “…Experimental results show that the ZM modifier significantly improves the dynamic stability and rutting resistance of the mixture, with dynamic stability increasing to 5245 and rut depth decreasing to 2.26 mm at a dosage of 0.5%. The low-temperature flexural strain increases while the bending stiffness decreases, indicating improved crack resistance. …”
  9. 37649

    Rutting test machine. by Yining Wang (432154)

    Published 2025
    “…Experimental results show that the ZM modifier significantly improves the dynamic stability and rutting resistance of the mixture, with dynamic stability increasing to 5245 and rut depth decreasing to 2.26 mm at a dosage of 0.5%. The low-temperature flexural strain increases while the bending stiffness decreases, indicating improved crack resistance. …”
  10. 37650

    Basic performance indicators of base asphalt. by Yining Wang (432154)

    Published 2025
    “…Experimental results show that the ZM modifier significantly improves the dynamic stability and rutting resistance of the mixture, with dynamic stability increasing to 5245 and rut depth decreasing to 2.26 mm at a dosage of 0.5%. The low-temperature flexural strain increases while the bending stiffness decreases, indicating improved crack resistance. …”
  11. 37651

    Rutting specimen. by Yining Wang (432154)

    Published 2025
    “…Experimental results show that the ZM modifier significantly improves the dynamic stability and rutting resistance of the mixture, with dynamic stability increasing to 5245 and rut depth decreasing to 2.26 mm at a dosage of 0.5%. The low-temperature flexural strain increases while the bending stiffness decreases, indicating improved crack resistance. …”
  12. 37652

    Orthogonal experimental design. by Yining Wang (432154)

    Published 2025
    “…Experimental results show that the ZM modifier significantly improves the dynamic stability and rutting resistance of the mixture, with dynamic stability increasing to 5245 and rut depth decreasing to 2.26 mm at a dosage of 0.5%. The low-temperature flexural strain increases while the bending stiffness decreases, indicating improved crack resistance. …”
  13. 37653

    Immersion Marshall test results. by Yining Wang (432154)

    Published 2025
    “…Experimental results show that the ZM modifier significantly improves the dynamic stability and rutting resistance of the mixture, with dynamic stability increasing to 5245 and rut depth decreasing to 2.26 mm at a dosage of 0.5%. The low-temperature flexural strain increases while the bending stiffness decreases, indicating improved crack resistance. …”
  14. 37654
  15. 37655
  16. 37656

    DataSheet_1_Astragalus Polysaccharides Inhibits Tumorigenesis and Lipid Metabolism Through miR-138-5p/SIRT1/SREBP1 Pathway in Prostate Cancer.doc by Shanqi Guo (8799437)

    Published 2020
    “…<p>Astragalus polysaccharides (APS) is a traditional Chinese medicine and have been proved to involve in multiple biological processes, including inflammation, metabolism, and carcinogenics. …”
  17. 37657

    Table_1_Fluorination Induced Donor to Acceptor Transformation in A1–D–A2–D–A1-Type Photovoltaic Small Molecules.DOCX by Ruimin Zhou (1494670)

    Published 2018
    “…The M-0F exhibited the highest efficiency of 5.99% as a donor in fullerene-containing system and the lowest efficiency of 0.58% as an acceptor in fullerene-free system. …”
  18. 37658

    Simultaneous Hypoxia and Low Extracellular pH Suppress Overall Metabolic Rate and Protein Synthesis In Vitro by Brita Singers Sørensen (783581)

    Published 2015
    “…This occurs due to an aberrant vasculature as well as high rates of glycolysis and lactate production in tumor cells even in the presence of oxygen (the Warburg effect), which weakens the spatial linkage between hypoxia and acidosis.</p><p>Methods</p><p>Five different human squamous cell carcinoma cell lines (SiHa, FaDu<sub>DD</sub>, UTSCC5, UTSCC14 and UTSCC15) were treated with hypoxia, acidosis (pH 6.3), or a combination, and gene expression analyzed using microarray. …”
  19. 37659

    High-Pressure Control of Vanadium Self-Intercalation and Enhanced Metallic Properties in 1<i>T</i>‑V<sub>1+<i>x</i></sub>S<sub>2</sub> Single Crystals by Hicham Moutaabbid (2412439)

    Published 2016
    “…By means of high-pressure synthesis in the 4–6 GPa range, we report on the successful growth of high-quality 1<i>T</i>-V<sub>1+<i>x</i></sub>S<sub>2</sub> single crystals with controlled concentration, <i>x</i> = 0.09–0.17, of self-intercalated V atoms in the van der Waals gap. …”
  20. 37660

    High-Pressure Control of Vanadium Self-Intercalation and Enhanced Metallic Properties in 1<i>T</i>‑V<sub>1+<i>x</i></sub>S<sub>2</sub> Single Crystals by Hicham Moutaabbid (2412439)

    Published 2016
    “…By means of high-pressure synthesis in the 4–6 GPa range, we report on the successful growth of high-quality 1<i>T</i>-V<sub>1+<i>x</i></sub>S<sub>2</sub> single crystals with controlled concentration, <i>x</i> = 0.09–0.17, of self-intercalated V atoms in the van der Waals gap. …”