    SEM image of the B0P0 mixture. by Jie Liu (15128)

    Published 2025
    “…The results indicate that the optimal combination was 0.1% volume content of 12-mm-long basalt fibers and 1.0% mass content of polycarboxylate superplasticizer, which yielded a compressive strength of 13.3 MPa and a splitting tensile strength of 1.14 MPa at 28 days. …”
  6. 6
  7. 7
  8. 8
  9. 9
  10. 10
  11. 11
  12. 12
  13. 13
  14. 14

    SEM image of the B3P0 mixture. by Jie Liu (15128)

    Published 2025
    “…The results indicate that the optimal combination was 0.1% volume content of 12-mm-long basalt fibers and 1.0% mass content of polycarboxylate superplasticizer, which yielded a compressive strength of 13.3 MPa and a splitting tensile strength of 1.14 MPa at 28 days. …”
  15. 15

    SEM image of the B0P3 mixture. by Jie Liu (15128)

    Published 2025
    “…The results indicate that the optimal combination was 0.1% volume content of 12-mm-long basalt fibers and 1.0% mass content of polycarboxylate superplasticizer, which yielded a compressive strength of 13.3 MPa and a splitting tensile strength of 1.14 MPa at 28 days. …”