يعرض 21 - 40 نتائج من 432 نتيجة بحث عن '(( greater increase ) OR ((((( steel decrease ) OR ( link decrease ))) OR ( sec decrease ))))*', وقت الاستعلام: 0.13s تنقيح النتائج
  1. 21
  2. 22

    Critical Review of Steel Column Base Plate Design Codes and Their Relevance to United Arab Emirates حسب SREENIVASAN, SREEJU

    منشور في 2019
    "…One of which the steel column base plate connection that would perform adequately for the specified demand. …"
    احصل على النص الكامل
  3. 23

    Evaluation of the cementite morphology influence on the hydrogen induced crack nucleation and propagation path in carbon steels حسب Shabnam Karimi (19457575)

    منشور في 2022
    "…<p>The effect of cementite morphology on the crack initiation and growth path was studied using in situ electrochem-ical micro-cantilever bending (ECCB) technique under hydrogen (H) charging. Two carbon steels with lamellar cementite morphology (pearlitic microstructure) and spherical or broken lamellas cementite morphology (spheroidite microstructure), both with approximately the same carbon equivalent, were used in this study. …"
  4. 24

    Fracture Behavior of ASTM A633 steel plate specimens with edge crack at tensile test حسب Abi Shdid, Caesar

    منشور في 2017
    "…The tensile test is an important and widely used test to determine the mechanical properties of steel materials. In tensile test, a specimen is pulled and specimen deformation and applied load is recorded until its fracture to draw load-displacement curve. …"
    احصل على النص الكامل
    احصل على النص الكامل
    احصل على النص الكامل
    conferenceObject
  5. 25

    Enhancing the corrosion resistance of reinforcing steel under aggressive operational conditions using behentrimonium chloride حسب A. Bahgat Radwan (9631720)

    منشور في 2019
    "…In conclusion, this new inhibitor shows high corrosion inhibition efficiencies under different aggressive conditions and can be used in concrete to reduce the corrosion rate of reinforcing steel without decreasing the mechanical properties of the concrete.…"
  6. 26

    Evaluation of the durability and shielding properties of high-strength concrete incorporating locally available materials and carbon additives حسب Othman, Obaida

    منشور في 2026
    "…However, the addition of carbon materials along with steel fibers (FCLDUNE) decreased these strengths by 19.6 and 15%, and increased shrinkage and creep by 18 and 9%, respectively. …"
    احصل على النص الكامل
    article
  7. 27

    Do high energy-efficient buildings increase overheating risk in cold climates? Causes and mitigation measures required under recent and future climates حسب Mutasim Baba, Fuad

    منشور في 2022
    "…While without adequate ventilation, the overheating risk in high-energy-efficient buildings can be higher than old buildings, where decreasing wall and window U-values and infiltration rate has a greater contribution to the increase of indoor temperature, while decreasing window SHGC has a lower contribution to the decrease in indoor temperature compared to the case with adequate ventilation. …"
    احصل على النص الكامل
    احصل على النص الكامل
    احصل على النص الكامل
  8. 28
  9. 29
  10. 30

    Electrochemical and thermodynamic study on the corrosion performance of API X120 steel in 3.5% NaCl solution حسب Khuram Shahzad (575887)

    منشور في 2020
    "…The overall results revealed that PEI significantly decreases the corrosion rate of API X120 steel with inhibition efficiency of 94% at a concentration of 100 μmol L<sup>−1</sup>. …"
  11. 31
  12. 32
  13. 33
  14. 34
  15. 35
  16. 36

    Part II.: Dissimilar friction stir welding of nickel titanium shape memory alloy to stainless steel – microstructure, mechanical and corrosion behavior حسب Parker West (17268946)

    منشور في 2021
    "…<p dir="ltr">In the present work, nickel-titanium (NiTi) shape memory alloys (SMAs) is joined to 304 stainless steel (SS) using friction stir welding (FSW) using process parameters of 400 rpm and a constant tool translation speed of 75 mm/min. …"
  17. 37

    Biodegradable polysaccharide grafted polyacrylamide inhibitor for corrosion in CO<sub>2</sub>- saturated saline solution حسب Rem Jalab (11715205)

    منشور في 2023
    "…Lastly, potentiostatic testing of steel with AGGPAM at an applied potential of 50 mV illustrated surface protection and decreased current over a prolonged time. …"
  18. 38

    The Photocatalytic Degradation of 2,3,7,8-Tetrachlorodibenzo-p-Dioxin in the Presence of Silver–Titanium Based Catalysts حسب Samara, Fatin

    منشور في 2020
    "…Byproducts of degradation were evaluated using Gas chromatography/mass spectrometry (GC–MS), resulting in 2,3,7-trichlorodibenzo-p-dioxin, a lower chlorinated congener and less toxic, as the main degradation product. Enzyme Linked Immunosorbent Assay (ELISA) was used to evaluate the relative toxicity of the degradation byproducts were a decrease in optical density indicated that some products of degradation could be potentially more toxic than the parent TCDD. …"
    احصل على النص الكامل
    article
  19. 39

    Towards Industry 4.0 and Sustainable Manufacturing Applying Environmentally Friendly Machining of a Precipitation Hardened Stainless Steel Using Hot Turning Process حسب Mohammadjafar Hadad (17541345)

    منشور في 2023
    "…In this research, the conventional and hot turning of AISI630 hardened stainless steel have been investigated using PVD-(Ti,Al)N/(Al,Cr)<sub>2</sub>O<sub>3</sub> coated carbide cutting tools at various feed rates and cutting speeds. …"
  20. 40

    Theoretical and experimental insights into the C-steel aqueous corrosion inhibition at elevated temperatures in 1.0 M HCl via multi-carbonyl Gemini cationic surfactants حسب Nasser M. El-Basiony (18021631)

    منشور في 2023